Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.1 g/cm³ Show Supplier Material materials with Dichte of 10.1 g/cm³ |
Abmessung
Property | Value |
---|---|
Breite | 609.6 mm Show Supplier Material materials with Breite of 609.6 mm |
Dicke | 0.25 - 0.76 mm Show Supplier Material materials with Dicke of 0.25 - 0.76 mm |
Länge | 1981 mm Show Supplier Material materials with Länge of 1981 mm |
Dimensions | Available dimensions (width x length x thickness, mm x mm x mm): 609.6 x 1981.2 x 0.254; 609.6 x 1981.2 x 0.381; 609.6 x 1981.2 x 0.508; 609.6 x 1981.2 x 0.762 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Vickers | 23.0 °C | 270 [-] Show Supplier Material materials with Härte, Vickers of 270 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % | ||
Andere | 0.61 - 0.73 % Show Supplier Material materials with Andere of 0.61 - 0.73 % | as La₂O₃ | |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % | ||
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % | ||
Eisen | 5E-4 % Show Supplier Material materials with Eisen of 5E-4 % | ||
Kalium | 6E-4 % Show Supplier Material materials with Kalium of 6E-4 % | ||
Kohlenstoff | 1.3E-3 % Show Supplier Material materials with Kohlenstoff of 1.3E-3 % | ||
Kupfer | 2E-4 % Show Supplier Material materials with Kupfer of 2E-4 % | ||
Lanthan | 0.52 - 0.62 % Show Supplier Material materials with Lanthan of 0.52 - 0.62 % | as La | |
Molybdän | balance | ||
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % | ||
Silizium | 2E-4 % Show Supplier Material materials with Silizium of 2E-4 % | ||
Stickstoff | 1E-4 % Show Supplier Material materials with Stickstoff of 1E-4 % | ||
Wolfram | 0.02 % Show Supplier Material materials with Wolfram of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | This alloy is mostly machined to produce furnace components such as stranded and other wires, sintering and annealing boats or evaporator coils. In the lighting industry, molybdenum-lanthanum oxide is used, for example, for retaining and feed wires. |