Allgemein
Property | Value |
---|---|
Kornstruktur | Fine-grained, homogeneous |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.34E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.34E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 97 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 97 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.30E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.30E+7 S/m |
Chemical properties
Property | Value |
---|---|
Molybdän | balance |
Tantal | 10.75 % Show Supplier Material materials with Tantal of 10.75 % |
Technological properties
Property | ||
---|---|---|
Application areas | Thanks to its good adherence to glass and a high level of electrical conductivity, molybdenum is a popular material for electrode layers in thin-film transistors (TFT-LCD) and touch sensors (touch panels). |