Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.1 g/cm³ Show Supplier Material materials with Dichte of 10.1 g/cm³ |
Oberflächenrauigkeit | 0.15 μm Show Supplier Material materials with Oberflächenrauigkeit of 0.15 μm |
Abmessung
Property | Value |
---|---|
Breite | 1.5 - 10 mm Show Supplier Material materials with Breite of 1.5 - 10 mm |
Dicke | 0.02 - 0.04 mm Show Supplier Material materials with Dicke of 0.02 - 0.04 mm |
Dimensions | Available dimensions (width x thickness, mm x mm): 1.5 x 0.02; 2 x 0.025; 3 x 0.025; 4 x 0.025; 2 x 0.028; 2.5 x 0.028; 3 x 0.028; 4 x 0.028; 3 x 0.03; 4.8 x 0.033; 5 x 0.035; 6 x 0.035; 10 x 0.04 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Zugfestigkeit | 23.0 °C | 750 - 1000 MPa Show Supplier Material materials with Zugfestigkeit of 750 - 1000 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % | ||
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % | ||
Cerium | 0.08 % Show Supplier Material materials with Cerium of 0.08 % | as CeO₂ | |
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % | ||
Eisen | 5E-4 % Show Supplier Material materials with Eisen of 5E-4 % | ||
Kalium | 4E-4 % Show Supplier Material materials with Kalium of 4E-4 % | ||
Kohlenstoff | 1.3E-3 % Show Supplier Material materials with Kohlenstoff of 1.3E-3 % | ||
Kupfer | 2E-4 % Show Supplier Material materials with Kupfer of 2E-4 % | ||
Molybdän | balance | ||
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % | ||
Silizium | 2E-4 % Show Supplier Material materials with Silizium of 2E-4 % | ||
Stickstoff | 1E-4 % Show Supplier Material materials with Stickstoff of 1E-4 % | ||
Wolfram | 0.02 % Show Supplier Material materials with Wolfram of 0.02 % | ||
Yttrium | 0.47 - 0.6 % Show Supplier Material materials with Yttrium of 0.47 - 0.6 % | as Y-mixed oxide |
Technological properties
Property | ||
---|---|---|
Application areas | MY is primarily used in conductive ESS ribbons and in evaporation boats for applications in the field of coating technology and in the lighting industry. | |
Other | ESS (Elliptically Shaped for Sealing-in) Ribbon with tapered edges by etching. |