Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.15 g/cm³ Show Supplier Material materials with Dichte of 10.15 g/cm³ |
Oberflächenrauigkeit | 1 μm Show Supplier Material materials with Oberflächenrauigkeit of 1 μm |
Abmessung
Property | Value |
---|---|
Durchmesser | 4.75 mm Show Supplier Material materials with Durchmesser of 4.75 mm |
Länge | 300 - 1900 mm Show Supplier Material materials with Länge of 300 - 1900 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 6 x 300-3000; 6.35 x 300-3000; 8 x 300-3000; 10 x 100-2900; 12 x 100-3000; 15.875 x 100-1500; 19.05 x 100-1700 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 18 % Show Supplier Material materials with Dehnung of 18 % |
Härte, Vickers | 23.0 °C | 260 - 320 [-] Show Supplier Material materials with Härte, Vickers of 260 - 320 [-] |
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % |
Eisen | 5E-4 % Show Supplier Material materials with Eisen of 5E-4 % |
Kalium | 6E-4 % Show Supplier Material materials with Kalium of 6E-4 % |
Kupfer | 2E-4 % Show Supplier Material materials with Kupfer of 2E-4 % |
Molybdän | balance |
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % |
Sauerstoff | 0.01 % Show Supplier Material materials with Sauerstoff of 0.01 % |
Silizium | 2E-4 % Show Supplier Material materials with Silizium of 2E-4 % |
Stickstoff | 5E-4 % Show Supplier Material materials with Stickstoff of 5E-4 % |
Titan | 0.4 - 0.55 % Show Supplier Material materials with Titan of 0.4 - 0.55 % |
Wolfram | 0.02 % Show Supplier Material materials with Wolfram of 0.02 % |
Zirkonium | 0.06 - 0.12 % Show Supplier Material materials with Zirkonium of 0.06 - 0.12 % |
Technological properties
Property | ||
---|---|---|
Application areas | TZM is used in high-temperature applications involving demanding mechanical loads, for example in forging tools or as rotating anodes in X-ray tubes. The recommended temperatures of use are between 700 and 1400 °C. |