Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.1 g/cm³ Show Supplier Material materials with Dichte of 10.1 g/cm³ |
Abmessung
Property | Value |
---|---|
Breite | 400 mm Show Supplier Material materials with Breite of 400 mm |
Dicke | 10 - 20 mm Show Supplier Material materials with Dicke of 10 - 20 mm |
Länge | 600 mm Show Supplier Material materials with Länge of 600 mm |
Dimensions | Available dimensions (width x length x thickness, mm x mm x mm): 400 x 600 x 10; 400 x 600 x 20 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 10 % Show Supplier Material materials with Dehnung of 10 % |
Härte, Vickers | 23.0 °C | 220 - 320 [-] Show Supplier Material materials with Härte, Vickers of 220 - 320 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 600 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 600 MPa |
Zugfestigkeit | 23.0 °C | 650 MPa Show Supplier Material materials with Zugfestigkeit of 650 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % |
Eisen | 5E-4 % Show Supplier Material materials with Eisen of 5E-4 % |
Kalium | 6E-4 % Show Supplier Material materials with Kalium of 6E-4 % |
Kupfer | 2E-4 % Show Supplier Material materials with Kupfer of 2E-4 % |
Molybdän | balance |
Nickel | 1E-4 % Show Supplier Material materials with Nickel of 1E-4 % |
Sauerstoff | 0.01 % Show Supplier Material materials with Sauerstoff of 0.01 % |
Silizium | 2E-4 % Show Supplier Material materials with Silizium of 2E-4 % |
Stickstoff | 5E-4 % Show Supplier Material materials with Stickstoff of 5E-4 % |
Titan | 0.4 - 0.55 % Show Supplier Material materials with Titan of 0.4 - 0.55 % |
Wolfram | 0.02 % Show Supplier Material materials with Wolfram of 0.02 % |
Zirkonium | 0.06 - 0.12 % Show Supplier Material materials with Zirkonium of 0.06 - 0.12 % |
Technological properties
Property | ||
---|---|---|
Application areas | TZM is used in high-temperature applications involving demanding mechanical loads, for example in forging tools or as rotating anodes in X-ray tubes. The recommended temperatures of use are between 700 and 1400 °C. |