Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 19.3 g/cm³ Show Supplier Material materials with Dichte of 19.3 g/cm³ |
Neutronenabsorptionsquerschnitt | 23.0 °C | 0 m² Show Supplier Material materials with Neutronenabsorptionsquerschnitt of 0 m² |
Abmessung
Property | Value |
---|---|
Breite | 508 mm Show Supplier Material materials with Breite of 508 mm |
Dicke | 0.13 - 0.25 mm Show Supplier Material materials with Dicke of 0.13 - 0.25 mm |
Länge | 838.2 mm Show Supplier Material materials with Länge of 838.2 mm |
Dimensions | Available dimensions (width x length x thickness, mm x mm x mm): 508 x 838.2 x 0.127; 508 x 838.2 x 0.254 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Vickers | 23.0 °C | 500 [-] Show Supplier Material materials with Härte, Vickers of 500 [-] |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 3420 °C Show Supplier Material materials with Schmelzpunkt of 3420 °C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektronenaustrittsarbeit | 23.0 °C | 4.54 eV Show Supplier Material materials with Elektronenaustrittsarbeit of 4.54 eV |
Akustisch
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Blei | 1E-4 % Show Supplier Material materials with Blei of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % |
Eisen | 8E-4 % Show Supplier Material materials with Eisen of 8E-4 % |
Kalium | 1E-4 % Show Supplier Material materials with Kalium of 1E-4 % |
Kohlenstoff | 6E-4 % Show Supplier Material materials with Kohlenstoff of 6E-4 % |
Kupfer | 1E-4 % Show Supplier Material materials with Kupfer of 1E-4 % |
Molybdän | 1.2E-3 % Show Supplier Material materials with Molybdän of 1.2E-3 % |
Nickel | 2E-4 % Show Supplier Material materials with Nickel of 2E-4 % |
Sauerstoff | 2E-4 % Show Supplier Material materials with Sauerstoff of 2E-4 % |
Silizium | 1E-4 % Show Supplier Material materials with Silizium of 1E-4 % |
Stickstoff | 1E-4 % Show Supplier Material materials with Stickstoff of 1E-4 % |
Wolfram | 99.97 % Show Supplier Material materials with Wolfram of 99.97 % |