Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 19.2 g/cm³ Show Supplier Material materials with Dichte of 19.2 g/cm³ |
Neutronenabsorptionsquerschnitt | 23.0 °C | 0 m² Show Supplier Material materials with Neutronenabsorptionsquerschnitt of 0 m² |
Abmessung
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Vickers | 23.0 °C | 550 [-] Show Supplier Material materials with Härte, Vickers of 550 [-] |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 3420 °C Show Supplier Material materials with Schmelzpunkt of 3420 °C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektronenaustrittsarbeit | 23.0 °C | 4.54 eV Show Supplier Material materials with Elektronenaustrittsarbeit of 4.54 eV |
Akustisch
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Blei | 1E-4 % Show Supplier Material materials with Blei of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % |
Eisen | 8E-4 % Show Supplier Material materials with Eisen of 8E-4 % |
Kalium | 1E-4 % Show Supplier Material materials with Kalium of 1E-4 % |
Kohlenstoff | 6E-4 % Show Supplier Material materials with Kohlenstoff of 6E-4 % |
Kupfer | 1E-4 % Show Supplier Material materials with Kupfer of 1E-4 % |
Molybdän | 1.2E-3 % Show Supplier Material materials with Molybdän of 1.2E-3 % |
Nickel | 2E-4 % Show Supplier Material materials with Nickel of 2E-4 % |
Sauerstoff | 2E-4 % Show Supplier Material materials with Sauerstoff of 2E-4 % |
Silizium | 1E-4 % Show Supplier Material materials with Silizium of 1E-4 % |
Wolfram | 99.97 % Show Supplier Material materials with Wolfram of 99.97 % |
Technological properties