Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 19.1 g/cm³ Show Supplier Material materials with Dichte of 19.1 g/cm³ |
Neutronenabsorptionsquerschnitt | 23.0 °C | 0 m² Show Supplier Material materials with Neutronenabsorptionsquerschnitt of 0 m² |
Oberflächenrauigkeit | 1 μm Show Supplier Material materials with Oberflächenrauigkeit of 1 μm |
Abmessung
Property | Value |
---|---|
Durchmesser | 2 - 25.4 mm Show Supplier Material materials with Durchmesser of 2 - 25.4 mm |
Länge | 300 - 2900 mm Show Supplier Material materials with Länge of 300 - 2900 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 2 x 500-2900; 2.54 x 500-2900; 3 x 500-2900; 3.175 x 500-2900; 4 x 500-2300; 4.75 x 500-2400; 5 x 500-2400; 6 x 500-2400; 6.35 x 500-2400; 8 x 500-2000; 10 x 500-2700; 12 x 300-1800; 12.7 x 300-1600; 14 x 300-1300; 16 x 300-1600; 18 x 300-2200; 19.05 x 300-1800; 20 x 300-1700; 25 x 300-2400; 25.4 x 300-2300 |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 3420 °C Show Supplier Material materials with Schmelzpunkt of 3420 °C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektronenaustrittsarbeit | 23.0 °C | 4.54 eV Show Supplier Material materials with Elektronenaustrittsarbeit of 4.54 eV |
Akustisch
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Blei | 1E-4 % Show Supplier Material materials with Blei of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % |
Eisen | 8E-4 % Show Supplier Material materials with Eisen of 8E-4 % |
Kalium | 1E-4 % Show Supplier Material materials with Kalium of 1E-4 % |
Kohlenstoff | 6E-4 % Show Supplier Material materials with Kohlenstoff of 6E-4 % |
Kupfer | 1E-4 % Show Supplier Material materials with Kupfer of 1E-4 % |
Molybdän | 1.2E-3 % Show Supplier Material materials with Molybdän of 1.2E-3 % |
Nickel | 2E-4 % Show Supplier Material materials with Nickel of 2E-4 % |
Sauerstoff | 2E-4 % Show Supplier Material materials with Sauerstoff of 2E-4 % |
Silizium | 1E-4 % Show Supplier Material materials with Silizium of 1E-4 % |
Stickstoff | 1E-4 % Show Supplier Material materials with Stickstoff of 1E-4 % |
Wolfram | 99.97 % Show Supplier Material materials with Wolfram of 99.97 % |
Technological properties
Property | ||
---|---|---|
Application areas | Tungsten rods are mainly used in the lighting industry and high temperature furnace construction. |