Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 17.1 g/cm³ Show Supplier Material materials with Dichte of 17.1 g/cm³ |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 22.0 °C | 6.4E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.4E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 195 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 195 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Kupfer | balance |
Wolfram | 10 % Show Supplier Material materials with Wolfram of 10 % |
Technological properties
Property | ||
---|---|---|
Application areas | WCu is used for the construction of high-voltage circuit breakers (marketed under the name Elmet®) and for erosion electrodes (marketed under the name Sparkal®). WCu composites are also used as base plates and heat spreaders in radar technology, optoelectronics and high frequency electronics. |