Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
Tungsten-Rhenium Alloy (WRe26)
To obtain greater ductility and a lower brittle-to-ductile transition temperature, tungsten is alloyed with rhenium. Moreover, tungsten-rhenium has a higher recrystallization temperature and better creep resistance.
Diese Materialdaten wurden von Plansee zur Verfügung gestellt
All categories
Base plates for semiconductors
Components for epitaxial growth processes
Cylinders for hot isostatic pressing (HIP)
Electrodes for resistance welding made of tungsten and molybdenum
Heating elements for MOCVD
Lead replacement for X-ray shielding
Molybdenum sputtering targets
Nozzles for the production of wool and fibers
Plansee’s newly patented coating material pushing boundaries in sputtering target efficiency
Tungsten Alloy Balancing Weights
Tungsten, molybdenum and tantalum for evaporation coils
Chemical properties
Property | Value |
---|---|
Rhenium | 26 % Show Supplier Material materials with Rhenium of 26 % |
Wolfram | balance |
Technological properties
Property | ||
---|---|---|
Application areas | The WRe standard compositions are used as material for thermoelements in applications of over 2000 °C. This material is also used in the aviation and aerospace industries. |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.