Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.57 g/cm³ Show Supplier Material materials with Dichte of 1.57 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Moisture absorption of 0.06 % | ISO 62 | (23°C / 50% RH) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 175 MPa Show Supplier Material materials with Biegefestigkeit of 175 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 10.5 GPa Show Supplier Material materials with Biegemodul of 10.5 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 1.3 % Show Supplier Material materials with Dehnung of 1.3 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 12 GPa Show Supplier Material materials with Elastizitätsmodul of 12 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 58 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 58 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 391 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 391 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 24 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 24 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 126 MPa Show Supplier Material materials with Zugfestigkeit of 126 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 275 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 275 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 258 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 258 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.2E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Relative temperature index, electrical | 220 °C Show Supplier Material materials with Relative temperature index, electrical of 220 °C | UL 746B | |||
Relative temperature index, mechanical impact | 200 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 200 °C | UL 746B | |||
Relative temperature index, mechanical strength | 220 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 220 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 258 - 275 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 258 - 275 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 4.5E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 4.5E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101283822- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101283821- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.45mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 4 |
High Volt Arc Track Rate | 23.0 °C | 1 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 1 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 1 |
Kriechstromfestigkeit | 23.0 °C | 4 V Show Supplier Material materials with Kriechstromfestigkeit of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Semiconductor | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |