Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Korngröße | 10.0 μm Show Supplier Material materials with Korngröße of 10.0 μm | ||
Permeabilitätskoeffizient | 20 °C | 0.25 cm²/s Show Supplier Material materials with Permeabilitätskoeffizient of 0.25 cm²/s | |
Porosität | 14.0 % Show Supplier Material materials with Porosität of 14.0 % | open porosity | |
Schüttdichte | 1.77 g/cm³ Show Supplier Material materials with Schüttdichte of 1.77 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 50 MPa Show Supplier Material materials with Biegefestigkeit of 50 MPa | |
Druckfestigkeit | 110 MPa Show Supplier Material materials with Druckfestigkeit of 110 MPa | |
Elastizitätsmodul | 10.5 GPa Show Supplier Material materials with Elastizitätsmodul of 10.5 GPa | Dynamic Modulus |
Hardness, Rockwell | 70.0 [-] Show Supplier Material materials with Hardness, Rockwell of 70.0 [-] | 5/100 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 0.02 % Show Supplier Material materials with Aschegehalt of 0.02 % | ||
Koeffizient der thermischen Ausdehnung | 4.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.2e-06 1/K | @20-200°C | |
Wärmeleitfähigkeit | 20 °C | 95 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 95 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | Metallurgical applications e.g. continuous casting, crucibles, sintering molds, etc. | |
Processing methods | Isostatically pressed |