Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 25 % Show Supplier Material materials with Dehnung of 25 % |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa |
Streckgrenze | 23.0 °C | 215 - 235 MPa Show Supplier Material materials with Streckgrenze of 215 - 235 MPa |
Zugfestigkeit | 23.0 °C | 375 - 500 MPa Show Supplier Material materials with Zugfestigkeit of 375 - 500 MPa |
Chemical properties
Property | Value |
---|---|
Eisen | Balance |
Kohlenstoff | 0.17 % Show Supplier Material materials with Kohlenstoff of 0.17 % |
Mangan | 1.4 % Show Supplier Material materials with Mangan of 1.4 % |
Phosphor | 0.05 % Show Supplier Material materials with Phosphor of 0.05 % |
Schwefel | 0.045 % Show Supplier Material materials with Schwefel of 0.045 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |