Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 14 % Show Supplier Material materials with Dehnung of 14 % |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa |
Streckgrenze | 23.0 °C | 345 MPa Show Supplier Material materials with Streckgrenze of 345 MPa |
Zugfestigkeit | 23.0 °C | 490 - 680 MPa Show Supplier Material materials with Zugfestigkeit of 490 - 680 MPa |
Chemical properties
Property | Value |
---|---|
Eisen | Balance |
Kohlenstoff | 0.2 % Show Supplier Material materials with Kohlenstoff of 0.2 % |
Mangan | 1.6 % Show Supplier Material materials with Mangan of 1.6 % |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Supplier Material materials with Schwefel of 0.035 % |
Silizium | 0.55 % Show Supplier Material materials with Silizium of 0.55 % |