Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.4 g/cm³ Show Supplier Material materials with Dichte of 8.4 g/cm³ |
Mechanisch
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.4 % Show Supplier Material materials with Aluminium of 0.4 % | |
Chrom | 20 - 23 % Show Supplier Material materials with Chrom of 20 - 23 % | |
Eisen | 5 % Show Supplier Material materials with Eisen of 5 % | |
Kohlenstoff | 0.1 % Show Supplier Material materials with Kohlenstoff of 0.1 % | |
Kupfer | 0.5 % Show Supplier Material materials with Kupfer of 0.5 % | |
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % | |
Molybdän | 8 - 10 % Show Supplier Material materials with Molybdän of 8 - 10 % | |
Nickel | 58 % Show Supplier Material materials with Nickel of 58 % | |
Niobium | 3.15 - 4.15 % Show Supplier Material materials with Niobium of 3.15 - 4.15 % | plus Hydrogen |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | |
Titan | 0.4 % Show Supplier Material materials with Titan of 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | 1. The organic chemical process parts contain chloride, especially in the use of acid chloride catalyst. 2. Absorption tower, re-heater, gas import board, fan, blender, fair water fin, flue and so on for using in flue gas desulfurization system. 3. The equipment and parts in the use of acidic gas environments. 4. Sulfur acid cooling |