Abmessung
Property | Value | Comment |
---|---|---|
Breite | 205 - 800 mm Show Supplier Material materials with Breite of 205 - 800 mm | |
Dicke | 800 mm Show Supplier Material materials with Dicke of 800 mm | max. |
Durchmesser | 20 - 800 mm Show Supplier Material materials with Durchmesser of 20 - 800 mm | |
Länge | 2000 - 5800 mm Show Supplier Material materials with Länge of 2000 - 5800 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | Typical for Steels |
Härte, Rockwell C | 23.0 °C | 64 - 65 [-] Show Supplier Material materials with Härte, Rockwell C of 64 - 65 [-] | Quenched |
Chemical properties
Property | Value |
---|---|
Chrom | 11.5 - 13 % Show Supplier Material materials with Chrom of 11.5 - 13 % |
Eisen | Balance |
Kohlenstoff | 2 - 2.3 % Show Supplier Material materials with Kohlenstoff of 2 - 2.3 % |
Mangan | 0.4 % Show Supplier Material materials with Mangan of 0.4 % |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % |