Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Abmessung
Property | Value | Comment |
---|---|---|
Breite | 10 - 2500 mm Show Supplier Material materials with Breite of 10 - 2500 mm | |
Dicke | 800 mm Show Supplier Material materials with Dicke of 800 mm | max. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | 23.0 °C | 40 - 42 J Show Supplier Material materials with Charpy impact energy, V-notch of 40 - 42 J | |
Dehnung | 23.0 °C | 10 - 12 % Show Supplier Material materials with Dehnung of 10 - 12 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | Typical for Steels |
Härte, Rockwell C | 23.0 °C | 54 - 60 [-] Show Supplier Material materials with Härte, Rockwell C of 54 - 60 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Supplier Material materials with Poissonzahl of 0.29 [-] | Typical for Steels |
Streckgrenze | 23.0 °C | 510 - 835 MPa Show Supplier Material materials with Streckgrenze of 510 - 835 MPa | |
Zugfestigkeit | 23.0 °C | 740 - 1270 MPa Show Supplier Material materials with Zugfestigkeit of 740 - 1270 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.9 - 1.2 % Show Supplier Material materials with Chrom of 0.9 - 1.2 % |
Eisen | Balance |
Kohlenstoff | 0.38 - 0.41 % Show Supplier Material materials with Kohlenstoff of 0.38 - 0.41 % |
Mangan | 0.5 - 0.8 % Show Supplier Material materials with Mangan of 0.5 - 0.8 % |
Molybdän | 0.15 - 0.3 % Show Supplier Material materials with Molybdän of 0.15 - 0.3 % |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % |
Schwefel | 0.035 % Show Supplier Material materials with Schwefel of 0.035 % |
Silizium | 0.15 - 0.4 % Show Supplier Material materials with Silizium of 0.15 - 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Turbines,Fasteners General,Steel Bars & Rods,Burners & Boilers,Gears,Shafts,Other Valves,Bolts,Nuts,Pressure Vessels,Iron & Steel Pipes |