Abmessung
Property | Value | Comment |
---|---|---|
Breite | 205 - 800 mm Show Supplier Material materials with Breite of 205 - 800 mm | |
Dicke | 800 mm Show Supplier Material materials with Dicke of 800 mm | max. |
Durchmesser | 20 - 800 mm Show Supplier Material materials with Durchmesser of 20 - 800 mm | |
Länge | 300 - 5800 mm Show Supplier Material materials with Länge of 300 - 5800 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | Typical for Steels |
Härte, Rockwell C | 23.0 °C | 62 - 66 [-] Show Supplier Material materials with Härte, Rockwell C of 62 - 66 [-] | Quenched |
Chemical properties
Property | Value |
---|---|
Chrom | 4.75 - 5.5 % Show Supplier Material materials with Chrom of 4.75 - 5.5 % |
Eisen | Balance |
Kohlenstoff | 0.33 - 0.43 % Show Supplier Material materials with Kohlenstoff of 0.33 - 0.43 % |
Mangan | 0.2 - 0.5 % Show Supplier Material materials with Mangan of 0.2 - 0.5 % |
Molybdän | 1.1 - 1.6 % Show Supplier Material materials with Molybdän of 1.1 - 1.6 % |
Nickel | 1.4 - 1.8 % Show Supplier Material materials with Nickel of 1.4 - 1.8 % |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 0.8 - 1.2 % Show Supplier Material materials with Silizium of 0.8 - 1.2 % |
Vanadium | 0.3 - 0.6 % Show Supplier Material materials with Vanadium of 0.3 - 0.6 % |