Abmessung
Property | Value |
---|---|
Breite | 80 - 1000 mm Show Supplier Material materials with Breite of 80 - 1000 mm |
Dicke | 20 - 400 mm Show Supplier Material materials with Dicke of 20 - 400 mm |
Durchmesser | 50 - 500 mm Show Supplier Material materials with Durchmesser of 50 - 500 mm |
Länge | 2000 - 5800 mm Show Supplier Material materials with Länge of 2000 - 5800 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | Typical for Steels |
Härte, Brinell | 23.0 °C | 248 [-] Show Supplier Material materials with Härte, Brinell of 248 [-] | Annealed |
Härte, Rockwell C | 23.0 °C | 60 - 62 [-] Show Supplier Material materials with Härte, Rockwell C of 60 - 62 [-] | Quenched |
Chemical properties
Property | Value |
---|---|
Chrom | 4.75 - 5.5 % Show Supplier Material materials with Chrom of 4.75 - 5.5 % |
Eisen | Balance |
Kohlenstoff | 0.95 - 1.05 % Show Supplier Material materials with Kohlenstoff of 0.95 - 1.05 % |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % |
Molybdän | 0.9 - 1.4 % Show Supplier Material materials with Molybdän of 0.9 - 1.4 % |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % |
Vanadium | 0.15 - 0.5 % Show Supplier Material materials with Vanadium of 0.15 - 0.5 % |