Abmessung
Property | Value |
---|---|
Durchmesser | 28.1 - 82.55 mm Show Supplier Material materials with Durchmesser of 28.1 - 82.55 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 17 % Show Supplier Material materials with Dehnung of 17 % |
Härte, Brinell | 23.0 °C | 250 [-] Show Supplier Material materials with Härte, Brinell of 250 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 620 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 620 MPa |
Zugfestigkeit | 23.0 °C | 900 MPa Show Supplier Material materials with Zugfestigkeit of 900 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 2.3 - 3.15 % Show Supplier Material materials with Aluminium of 2.3 - 3.15 % | ||
Andere | 63 % Show Supplier Material materials with Andere of 63 % | Ni+Co | |
Eisen | 2 % Show Supplier Material materials with Eisen of 2 % | ||
Kohlenstoff | 0.25 % Show Supplier Material materials with Kohlenstoff of 0.25 % | ||
Kupfer | 27 - 33 % Show Supplier Material materials with Kupfer of 27 - 33 % | ||
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | ||
Nickel | Balance | ||
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | ||
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % | ||
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | ||
Titan | 0.35 - 0.85 % Show Supplier Material materials with Titan of 0.35 - 0.85 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical area of usage is pump shafts and oil well tools. | |
Heat Treatment | Solution annealing: 980 – 1040°C. Age hardened: 540 – 600°C. | |
Welding | Very good |