Other Components For Electrical Equipment

Quick Comparison

Wrought Copper High Copper Alloy

AMPCOLOY® 940 Sand castings

Geliefert von:

AMPCO METAL

Wrought Copper High Copper Alloy

AMPCOLOY® 972 Extruded and drawn rounds

Geliefert von:

AMPCO METAL

Polypropylen (PP)

DuraSense Pure S40 Food

Geliefert von:

Stora Enso Biocomposites

Polypropylen (PP)

DuraSense Pure L40 Food

Geliefert von:

Stora Enso Biocomposites

Polypropylen (PP)

DuraSense Pure S50 Food

Geliefert von:

Stora Enso Biocomposites

Polypropylen (PP)

DuraSense Pure L50 Food

Geliefert von:

Stora Enso Biocomposites

Polypropylen (PP)

DuraSense Pure 30 Food

Geliefert von:

Stora Enso Biocomposites

Polypropylen (PP)

Eco PP S40 Flex K Food

Geliefert von:

Stora Enso Biocomposites

Polypropylen (PP)

DuraSense Eco PP 30 Food

Geliefert von:

Stora Enso Biocomposites
Seite 1 von 2