Allgemein
Property | Value |
---|---|
Dichte | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 20 °C | 200 GPa Show Supplier Material materials with Elastizitätsmodul of 200 GPa |
100 °C | 194 GPa Show Supplier Material materials with Elastizitätsmodul of 194 GPa | |
200 °C | 186 GPa Show Supplier Material materials with Elastizitätsmodul of 186 GPa | |
300 °C | 180 GPa Show Supplier Material materials with Elastizitätsmodul of 180 GPa | |
Zugfestigkeit | 650.0 - 880.0 MPa Show Supplier Material materials with Zugfestigkeit of 650.0 - 880.0 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.000013 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000013 1/K | 20 to 100°C | |
0.000014 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000014 1/K | 20 to 300°C | ||
0.000135 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000135 1/K | 20 to 200°C | ||
Spezifische Wärmekapazität | 20 °C | 500 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | |
100 °C | 530 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 530 J/(kg·K) | ||
200 °C | 560 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 560 J/(kg·K) | ||
300 °C | 590 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 590 J/(kg·K) | ||
Wärmeleitfähigkeit | 20 °C | 15 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 15 W/(m·K) | |
100 °C | 16 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 16 W/(m·K) | ||
200 °C | 17 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 17 W/(m·K) | ||
300 °C | 18 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 18 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20 °C | 0.0000008 Ω·m Show Supplier Material materials with spezifischer Widerstand of 0.0000008 Ω·m |
100 °C | 0.00000085 Ω·m Show Supplier Material materials with spezifischer Widerstand of 0.00000085 Ω·m | |
200 °C | 0.0000009 Ω·m Show Supplier Material materials with spezifischer Widerstand of 0.0000009 Ω·m | |
300 °C | 0.000001 Ω·m Show Supplier Material materials with spezifischer Widerstand of 0.000001 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 22.0 - 24.0 % Show Supplier Material materials with Chrom of 22.0 - 24.0 % | |
Kohlenstoff | 0.03 Show Supplier Material materials with Kohlenstoff of 0.03 | max. |
Kupfer | 0.1 - 0.6000000000000001 % Show Supplier Material materials with Kupfer of 0.1 - 0.6000000000000001 % | |
Mangan | 2.0 Show Supplier Material materials with Mangan of 2.0 | max. |
Molybdän | 0.1 - 0.6000000000000001 % Show Supplier Material materials with Molybdän of 0.1 - 0.6000000000000001 % | |
Nickel | 3.5 - 5.5 % Show Supplier Material materials with Nickel of 3.5 - 5.5 % | |
Phosphor | 0.035 Show Supplier Material materials with Phosphor of 0.035 | max. |
Schwefel | 0.015 Show Supplier Material materials with Schwefel of 0.015 | max. |
Silizium | 1.0 Show Supplier Material materials with Silizium of 1.0 | max. |
Stickstoff | 0.05 - 0.2 % Show Supplier Material materials with Stickstoff of 0.05 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Hydraulic and pneumatic mechanisms | |
Corrosion properties | As UGICHROM® is "stainless in mass" there are no corrosion resistance problems over time, provided that the chosen grade is appropriate to the place of use. Passive layer: Stainless steels produce a very fine surface film of oxide consisting of chromium oxides and hydroxides a few Angströms thick. This oxide, commonly called a passive layer, protects the stainless steel against external attacks and gives it the property known as inoxidibility which guarantees the corrosion resistance of these alloys. The passive layer is an intrinsic part of the material, unlike the "Nickel-Chromium" coating deposited on carbon steels, which explains why stainless steel exhibits the basic corrosion resistance and adhesion advantages of chromium under harsh mechanical operating conditions (buckling). Once formed, this passive layer is completely stable since its thickness remains constant. The passive layer inhibits any exchange between the metal and the outside: in the event of damage to the material (scratch, cut, impact, drilling, deformation, etc.), it reforms spontaneously. This self-restructuring is also called "Repassivation". Choosing the most suitable grade: Only choosing the grade that is most appropriate to the operating environment increases the durability of hydraulic cylinders, depending on use. The figure on the right side of the material page shows how to obtain the best compromise between mechanical strength and corrosion resistance (see the chart on the right side of the material page). | |
Other | The mechanical properties of UGICHROM® are suitable for all hydraulic applications: Conditioning: The UGICHROM® product range offers a wide variety of conditioning options suitable for all customers' needs: Individual protection: Possibility of continuous ink jet marking on individual extruded plastic protection. Packaging: |