Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Austenitischer rostfreier Stahl
Sandvik 2RE10Geliefert von:
Alleima (formerly Sandvik Materials Technology)Martensitischer Edelstahl
UGI® 4062 solution annealed, hot rolled bars and wire rodGeliefert von:
UgitechAustenitischer rostfreier Stahl
EN 10088-1 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Ferritischer Edelstahl
DIN 17440 Grade X3CrTi17 soft annealed (+A)Ferritischer Edelstahl
DIN 17440 Grade X6CrAl13 soft annealed (+A)Ferritischer Edelstahl
EN 10088-1 Grade X3CrNb17 soft annealed (+A)Austenitischer rostfreier Stahl
EN 10088-1 Grade X1CrNi25-21 solution annealed (+AT)