Allgemein
Property | Value | Comment |
---|---|---|
Schichtdicke | 3.5 Show Supplier Material materials with Schichtdicke of 3.5 | |
Schichtnummer | 1.0 - 10.0 [-] Show Supplier Material materials with Schichtnummer of 1.0 - 10.0 [-] | ≤5 is 60%, ≤10 is 90% and >10 is 10%, using Raman |
Seitliche Flockengröße | 10000.0 Show Supplier Material materials with Seitliche Flockengröße of 10000.0 | Using SEM |
Mechanisch
Property | Value |
---|---|
Elastizitätsmodul | 1000.0 GPa Show Supplier Material materials with Elastizitätsmodul of 1000.0 GPa |
Zugfestigkeit | 13000.0 MPa Show Supplier Material materials with Zugfestigkeit of 13000.0 MPa |
Thermisch
Property | Value |
---|---|
Wärmeleitfähigkeit | 5000 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 5000 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Fluor | 1.0 % Show Supplier Material materials with Fluor of 1.0 % |
Kohlenstoff | 97.0 - 99.0 % Show Supplier Material materials with Kohlenstoff of 97.0 - 99.0 % |
Sauerstoff | 1.0 - 3.0 % Show Supplier Material materials with Sauerstoff of 1.0 - 3.0 % |
Schwefel | 1.0 % Show Supplier Material materials with Schwefel of 1.0 % |
Stickstoff | 0.6000000000000001 % Show Supplier Material materials with Stickstoff of 0.6000000000000001 % |
Technological properties
Property | ||
---|---|---|
Application areas | Being electrically conductive, thermally conductive and a highly effective mechanical reinforcer there are numerous potential applications for graphene such as: composites, energy, biomedical, membranes, coatings, sensors, electronics |