Allgemein
Property | Value | Comment |
---|---|---|
Schichtnummer | 1.0 - 100.0 [-] Show Supplier Material materials with Schichtnummer of 1.0 - 100.0 [-] | ≤5 is 18%, ≤10 is 73% and 10-100 is 27%, using Raman |
Seitliche Flockengröße | 26500.0 Show Supplier Material materials with Seitliche Flockengröße of 26500.0 | Using SEM |
Chemical properties
Property | Value |
---|---|
Fluor | 2.0 % Show Supplier Material materials with Fluor of 2.0 % |
Kohlenstoff | 93.0 - 99.0 % Show Supplier Material materials with Kohlenstoff of 93.0 - 99.0 % |
Sauerstoff | 1.0 - 5.0 % Show Supplier Material materials with Sauerstoff of 1.0 - 5.0 % |
Schwefel | 2.0 % Show Supplier Material materials with Schwefel of 2.0 % |
Stickstoff | 0.6000000000000001 % Show Supplier Material materials with Stickstoff of 0.6000000000000001 % |
Technological properties
Property | ||
---|---|---|
Application areas | Being electrically conductive, thermally conductive and a highly effective mechanical reinforcer there are numerous potential applications for graphene such as: composites, energy, biomedical, membranes, coatings, sensors, electronics |