Allgemein
Property | Value | Comment |
---|---|---|
Schichtnummer | 1.0 - 2.0 [-] Show Supplier Material materials with Schichtnummer of 1.0 - 2.0 [-] | Using AFM |
Seitliche Flockengröße | 4000.0 Show Supplier Material materials with Seitliche Flockengröße of 4000.0 | Using SEM/AFM |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 55.0 - 65.0 % Show Supplier Material materials with Kohlenstoff of 55.0 - 65.0 % |
Mangan | 3.0 % Show Supplier Material materials with Mangan of 3.0 % |
Sauerstoff | 28.0 - 38.0 % Show Supplier Material materials with Sauerstoff of 28.0 - 38.0 % |
Schwefel | 5.0 % Show Supplier Material materials with Schwefel of 5.0 % |
Stickstoff | 3.0 % Show Supplier Material materials with Stickstoff of 3.0 % |
Technological properties
Property | ||
---|---|---|
Application areas | li-ion batteries, fuel cells , battery electrodes, solar pv cells, electrically conductive inks, thermally conductive films and coatings, thermal interface materials, lightweight composites, concrete, metal -matrix composites, corrosion protection, barrier properties / permeation / mechanical performance | |
Color | Brown |