Allgemein
Property | Value |
---|---|
Schichtdicke | 0.003 Show Supplier Material materials with Schichtdicke of 0.003 |
Seitliche Flockengröße | 80.0 - 500.0 nm Show Supplier Material materials with Seitliche Flockengröße of 80.0 - 500.0 nm |
Elektrisch
Property | Value | Comment |
---|---|---|
Surface resistivity | 30.0 - 4000.0 Ω/sq Show Supplier Material materials with Surface resistivity of 30.0 - 4000.0 Ω/sq | Minimum for 80nm and Maximum for 2µm thickness |
Rheological Properties
Property | Value |
---|---|
Viskosität | 0.003 Pa·s Show Supplier Material materials with Viskosität of 0.003 Pa·s |
Technological properties
Property | ||
---|---|---|
Application areas | flexible electronics | |
Processing methods | Ink jet printing, Vacuum Filtration, Meyer Bar Coating - with a drying condition of 100℃ for 10 min |