Acero bajo en carbono
EN 10132-4 Grade C125S soft annealed or soft annealed and skin passed (+A or +A+LC)Acero bajo en carbono
EN 10132-4 Grade C125S quenched and tempered (+QT)Acero bajo en carbono
EN 10132-4 Grade C125S cold rolled (+CR)Acero bajo en carbono
EN 10132-4 Grade C125S quenched (+Q)Manganese Steel
SEW 395 Grade G-X120Mn13 solution heat-treated and quenchedAcero inoxidable martensítico
SEW 410 Grade G-X120Cr29 cast conditionAcero inoxidable ferrítico
SEW 410 Grade G-X120CrMo29-2 cast conditionPure/Low Nickel Alloy
DIN 17730 Grade G-Ni93C cast conditionAcero para herramientas y maquinaria
EN 10132-4 Grade 125Cr2 soft annealed or soft annealed and skin passed (+A or +A+LC)Acero para herramientas y maquinaria
ISO 4957 Grade 115CrV3 quenched (+Q)Acero bajo en carbono
ASTM A128 Grade FAcero para herramientas y maquinaria
ISO 4957 Grade S 10-4-3-10 quenched (+Q)Acero para herramientas y maquinaria
ISO 4957 Grade S 6-5-3 quenched (+Q)Acero inoxidable austenítico
ASTM A312 Grade S31272Acero para herramientas y maquinaria
EN 10132-4 Grade 125Cr2 quenched and tempered (+QT)Acero para herramientas y maquinaria
EN 10132-4 Grade 125Cr2 quenched (+Q)Acero para herramientas y maquinaria
ASTM A681 Grade Type A10 AnnealedAcero para herramientas y maquinaria
ASTM A681 Grade Type A3 Cold DrawnAcero para herramientas y maquinaria
ASTM A681 Grade Type F1 AnnealedAcero para herramientas y maquinaria
ASTM A681 Grade Type F1 Cold Drawn