Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.72 - 8 g/cm³ Show Material materials with Density of 7.72 - 8 g/cm³ | Typical for Tool And Machining Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 203 - 211 GPa Show Material materials with Elastic modulus of 203 - 211 GPa | Typical for Tool And Machining Steel |
Elongation A80 | 20.0 °C | 11 % Show Material materials with Elongation A80 of 11 % | |
Hardness, Brinell | 20.0 °C | 97 [-] Show Material materials with Hardness, Brinell of 97 [-] | |
Hardness, Vickers | 20.0 °C | 235 [-] Show Material materials with Hardness, Vickers of 235 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Tool And Machining Steel |
Shear modulus | 23.0 °C | 79 GPa Show Material materials with Shear modulus of 79 GPa | Typical for Tool And Machining Steel |
Tensile strength | 20.0 °C | 750 MPa Show Material materials with Tensile strength of 750 MPa | |
Yield strength Rp0.2 | 20.0 °C | 590 MPa Show Material materials with Yield strength Rp0.2 of 590 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K | Typical for Tool And Machining Steel |
Melting point | 1370 - 1425 °C Show Material materials with Melting point of 1370 - 1425 °C | Typical for Tool And Machining Steel | |
Specific heat capacity | 23.0 °C | 420 - 460 J/(kg·K) Show Material materials with Specific heat capacity of 420 - 460 J/(kg·K) | Typical for Tool And Machining Steel |
Thermal conductivity | 23.0 °C | 17 - 42 W/(m·K) Show Material materials with Thermal conductivity of 17 - 42 W/(m·K) | Typical for Tool And Machining Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 1.2 - 1.3 % Show Material materials with Carbon of 1.2 - 1.3 % |
Chromium | 0.4 - 0.6 % Show Material materials with Chromium of 0.4 - 0.6 % |
Manganese | 0.25 - 0.4 % Show Material materials with Manganese of 0.25 - 0.4 % |
Molybdenum | 0.1 % Show Material materials with Molybdenum of 0.1 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.15 - 0.35 % Show Material materials with Silicon of 0.15 - 0.35 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |