EN 10132-4 Grade C125S cold rolled (+CR)

Want to keep this datasheet? Save it now in your required format

Description

The steel C125S is used as cold rolled strip for springs and special applications in thicknesses of up to 6 mm and as tempered cold strip in thicknesses from 0.30 to 3.00 mm. The springs made of steel C125S are suitable for highly stressed tension springs, especially in the watch industry, as well as for pen nibs.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Low Carbon Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Low Carbon Steel

Hardness, Vickers

20.0 °C

325 [-]

Show Material materials with Hardness, Vickers of 325 [-]

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Low Carbon Steel

Shear modulus

23.0 °C

82 GPa

Show Material materials with Shear modulus of 82 GPa

Typical for Low Carbon Steel

Tensile strength

20.0 °C

1200 MPa

Show Material materials with Tensile strength of 1200 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.32E-5 - 1.38E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K

Typical for Low Carbon Steel

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Specific heat capacity

23.0 °C

465 J/(kg·K)

Show Material materials with Specific heat capacity of 465 J/(kg·K)

Typical for Low Carbon Steel

Thermal conductivity

23.0 °C

25 - 93 W/(m·K)

Show Material materials with Thermal conductivity of 25 - 93 W/(m·K)

Typical for Low Carbon Steel

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

1.43E-7 - 1.74E-7 Ω·m

Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m

Typical for Carbon Steel

Magnetic

PropertyValueComment

Curie temperature

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValue

Carbon

1.2 - 1.3 %

Show Material materials with Carbon of 1.2 - 1.3 %

Chromium

0.4 %

Show Material materials with Chromium of 0.4 %

Manganese

0.3 - 0.6 %

Show Material materials with Manganese of 0.3 - 0.6 %

Molybdenum

0.1 %

Show Material materials with Molybdenum of 0.1 %

Nickel

0.4 %

Show Material materials with Nickel of 0.4 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.15 - 0.35 %

Show Material materials with Silicon of 0.15 - 0.35 %

Sulfur

0.025 %

Show Material materials with Sulfur of 0.025 %

Do you have a technical question or need more information about this material?