Acero inoxidable austenítico
ASTM A276 Grade S20910 AnnealedCompuesto de matriz de aluminio
AlBeMet® AM162 Extruded (rod, Bar, Tube)Suministrada por:
Materion Brush GmbHAcero inoxidable austenítico
DIN 17440 Grade X2CrNiMoN17-13-3 solution heat-treated and quenchedNickel Chromium Iron Alloy
DIN 17744 Grade NiCr19NbMo precipitation hardened (+P)Acero inoxidable austenítico
DIN 17440 Grade X5CrNiMo17-12-2 solution heat-treated and quenchedAcero inoxidable endurecido por precipitación
UNS S45500 AnnealedNickel Chromium Alloy
DIN 17742 Grade NiCr15Fe soft annealed (+A)Acero inoxidable austenítico
EN 10028-7 Grade X5NiCrAlTi31-20 recrystallization annealed (+RA)Acero inoxidable austenítico
EN 10028-7 Grade X5NiCrAlTi31-20 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X5NiCrAlTi31-20 recrystallization annealed (+RA)Nickel Chromium Molybdenum Alloy
DIN 17744 Grade NiCr22Mo9Nb soft annealed (+A)Acero inoxidable austenítico
DIN 17460 Grade X5NiCrAlTi31-20 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X3CrNiCu19-9-2 solution annealed (+AT)Acero bajo en carbono
ASTM A1011 Grade CS Type BAcero inoxidable austenítico
EN 10222-5 Grade X3CrNiMo18-12-3 solution annealed (+AT)Acero bajo en carbono
AISI 1006 Cold DrawnAcero bajo en carbono
AISI 1008 Cold Drawn