General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.46 - 0.49 [-] Show Supplier Material materials with Coefficient of friction of 0.46 - 0.49 [-] | ||
Coefficient of friction, kinetic | 0.46 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.46 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.49 [-] Show Supplier Material materials with Coefficient of friction, static of 0.49 [-] | ASTM D 3702 Modified: Manual | |
Density | 23.0 °C | 1.55 g/cm³ Show Supplier Material materials with Density of 1.55 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.33 % Show Supplier Material materials with Moisture absorption of 0.33 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 9.9 GPa Show Supplier Material materials with Elastic modulus of 9.9 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2.5 % Show Supplier Material materials with Elongation of 2.5 % | ISO 527 | break |
Flexural modulus | 23.0 °C | 11.2 GPa Show Supplier Material materials with Flexural modulus of 11.2 GPa | ISO 178 |
Flexural strength | 23.0 °C | 285 MPa Show Supplier Material materials with Flexural strength of 285 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 12 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 117 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 117 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 70 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 70 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1035 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1035 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 6 J Show Supplier Material materials with Instrumented Impact, at Peak of 6 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 196 MPa Show Supplier Material materials with Tensile strength of 196 MPa | ISO 527 | break |
Thermal
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Washing Machine, Heavy Vehicles, Fuel Handling, Lawn/Garden, Electronic Components, Enclosures | |
Availability | Asia,Americas | |
Processing methods | Melt Temperature: 315 to 330.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |