Constante dieléctrica: 20 [-]

Quick Comparison

Polyamide 6 (PA6)

Akulon® K224-G6

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-G6-FC BK00001

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-G6-FC NA99001

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-HG6

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K227-XHG6

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-LG6 /E

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-G6U

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-HG6U

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-LG6U

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Polyamide 6 Reinforced with 30% Glass Fibre (PA6+GF30)

Suministrada por:

3 proveedores de Matmatch