Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® K224-G6-FC NA99001

This material data has been provided by DSM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.35 g/cm³

Show Supplier Material materials with Density of 1.35 g/cm³

dry

ISO 1183

Moisture absorption

1.9 %

Show Supplier Material materials with Moisture absorption of 1.9 %

dry

Sim. to ISO 62

Water absorption

6.3 %

Show Supplier Material materials with Water absorption of 6.3 %

dry

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

6 GPa

Show Supplier Material materials with Elastic modulus of 6 GPa

conditioned

ISO 527-1/-2

9.5 GPa

Show Supplier Material materials with Elastic modulus of 9.5 GPa

dry

ISO 527-1/-2

Elongation

3.5 %

Show Supplier Material materials with Elongation of 3.5 %

dry

ISO 527-1/-2

7 %

Show Supplier Material materials with Elongation of 7 %

conditioned

ISO 527-1/-2

Flexural modulus

8.6 GPa

Show Supplier Material materials with Flexural modulus of 8.6 GPa

dry

ISO 178

Flexural yield strength

235 MPa

Show Supplier Material materials with Flexural yield strength of 235 MPa

dry

ISO 178

Hardness, Shore D

85 [-]

Show Supplier Material materials with Hardness, Shore D of 85 [-]

dry

ISO 868

15s

Impact strength, Charpy notched

-30 °C

11 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m²

dry, conditioned

ISO 179/1eA

23 °C

12 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m²

dry

ISO 179/1eA

23 °C

25 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 25 kJ/m²

conditioned

ISO 179/1eA

Impact strength, Charpy unnotched

-30 °C

75 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 75 kJ/m²

dry, conditioned

ISO 179/1eU

23 °C

90 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m²

dry

ISO 179/1eU

23 °C

110 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 110 kJ/m²

conditioned

ISO 179/1eU

Tensile strength

110 MPa

Show Supplier Material materials with Tensile strength of 110 MPa

conditioned

ISO 527-1/-2

180 MPa

Show Supplier Material materials with Tensile strength of 180 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardThicknessPressureComment

Coefficient of thermal expansion

2e-07 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2e-07 1/K

dry

ISO 11359-1/-2

Parallel

7e-07 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 7e-07 1/K

dry

ISO 11359-1/-2

Normal

Flammability

HB

dry

IEC 60695-11-10

1.5 mm

UL recognition :Yes

Heat deflection temperature

200 °C

Show Supplier Material materials with Heat deflection temperature of 200 °C

dry

ISO 75-1/-2

2 MPa

220 °C

Show Supplier Material materials with Heat deflection temperature of 220 °C

dry

ISO 75-1/-2

0.45 MPa

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

dry

ISO 11357-1/-3

10°C/min

Relative temperature index, electrical

65 °C

Show Supplier Material materials with Relative temperature index, electrical of 65 °C

dry

UL746B

0.75 mm

Relative temperature index, mechanical impact

65 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C

dry

UL746B

0.75 mm

Relative temperature index, mechanical strength

65 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C

dry

UL746B

0.75 mm

Thermal diffusivity

1.12e-07 mm²/s

Show Supplier Material materials with Thermal diffusivity of 1.12e-07 mm²/s

dry

-

Electrical

PropertyValueConditionTesting StandardComment

Comparative tracking index

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

conditioned

IEC 60112

Dielectric constant

3.3 [-]

Show Supplier Material materials with Dielectric constant of 3.3 [-]

dry

IEC 62631-2-1

1MHz

3.5 [-]

Show Supplier Material materials with Dielectric constant of 3.5 [-]

dry

IEC 62631-2-1

100Hz

5 [-]

Show Supplier Material materials with Dielectric constant of 5 [-]

conditioned

IEC 62631-2-1

1MHz

20 [-]

Show Supplier Material materials with Dielectric constant of 20 [-]

conditioned

IEC 62631-2-1

100Hz

Dielectric strength

25 kV/mm

Show Supplier Material materials with Dielectric strength of 25 kV/mm

conditioned

IEC 60243-1

30 kV/mm

Show Supplier Material materials with Dielectric strength of 30 kV/mm

dry

IEC 60243-1

Dissipation factor

50 [-]

Show Supplier Material materials with Dissipation factor of 50 [-]

dry

IEC 62631-2-1

100Hz

150 [-]

Show Supplier Material materials with Dissipation factor of 150 [-]

dry

IEC 62631-2-1

1MHz

1200 [-]

Show Supplier Material materials with Dissipation factor of 1200 [-]

conditioned

IEC 62631-2-1

1MHz

3000 [-]

Show Supplier Material materials with Dissipation factor of 3000 [-]

conditioned

IEC 62631-2-1

100Hz

Surface resistivity

1e+14 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq

conditioned

IEC 62631-3-2

Volume resistivity

1e+11 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm

conditioned

IEC 62631-3-1

1e+13 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm

dry

IEC 62631-3-1

Rheological Properties

PropertyTemperatureValueConditionTesting StandardComment

Density of melt

1150 g/cm³

Show Supplier Material materials with Density of melt of 1150 g/cm³

dry

-

Melt mass-flow rate

240 °C

7.3 g/10min

Show Supplier Material materials with Melt mass-flow rate of 7.3 g/10min

dry

ISO 1133

Melt volume-flow rate

240 °C

6.4 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 6.4 cm³/10min

dry

ISO 1133

Shrinkage

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

dry

ISO 294-4

Parallel

0.9 %

Show Supplier Material materials with Shrinkage of 0.9 %

dry

ISO 294-4

Normal

Specific heat capacity melt

2110 J/(kg·K)

Show Supplier Material materials with Specific heat capacity melt of 2110 J/(kg·K)

dry

-

Thermal conductivity of melt

0.27 W/(m·K)

Show Supplier Material materials with Thermal conductivity of melt of 0.27 W/(m·K)

dry

-

Technological properties

Property
Certifications

Food Contact, Yellow Card Available

Fillers

30% Glass Fiber