Polyamide 6 Reinforced with 30% Glass Fibre (PA6+GF30)

Alternative and trade names
Zytel®, Ultramid®, Akulon®, Bergamid™, Durethan®, TECACOMP®, Novamid®, Orgalloy®, Radilon®
Want to keep this datasheet? Save it now in your required format

Description

Reinforced Polyamide 6 with 30% glass fiber. These materials are distinguished by:


  • high mechanical strength
  • hardness and rigidity
  • thermostability and resistance to hot lubricants and hot water
  • Parts made from them show dimensional stability and high creep strength.
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.31 - 1.37 g/cm³

    Show Material materials with Density of 1.31 - 1.37 g/cm³

    Mechanical

    PropertyValueComment

    Elastic modulus

    5.6 - 8.2 GPa

    Show Material materials with Elastic modulus of 5.6 - 8.2 GPa

    Elongation

    4.0 - 10.0 %

    Show Material materials with Elongation of 4.0 - 10.0 %

    Impact strength, Charpy notched

    15.0 - 45.0 kJ/m²

    Show Material materials with Impact strength, Charpy notched of 15.0 - 45.0 kJ/m²

    Impact strength, Charpy unnotched

    80 kJ/m²

    Show Material materials with Impact strength, Charpy unnotched of 80 kJ/m²

    120 kJ/m²

    Show Material materials with Impact strength, Charpy unnotched of 120 kJ/m²

    Tensile strength

    90.0 - 135.0 MPa

    Show Material materials with Tensile strength of 90.0 - 135.0 MPa

    at 4-10% strain

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    2e-05 - 0.00011 1/K

    Show Material materials with Coefficient of thermal expansion of 2e-05 - 0.00011 1/K

    Melting point

    220.0 - 225.0 °C

    Show Material materials with Melting point of 220.0 - 225.0 °C

    Specific heat capacity

    1500 J/(kg·K)

    Show Material materials with Specific heat capacity of 1500 J/(kg·K)

    Thermal conductivity

    0.24 W/(m·K)

    Show Material materials with Thermal conductivity of 0.24 W/(m·K)

    Flammability

    UL 94 HB

    Electrical

    PropertyValue

    Dielectric constant

    4 [-]

    Show Material materials with Dielectric constant of 4 [-]

    20 [-]

    Show Material materials with Dielectric constant of 20 [-]

    Electrical resistivity

    1000000000.0 - 10000000000000.0 Ω·m

    Show Material materials with Electrical resistivity of 1000000000.0 - 10000000000000.0 Ω·m

    Optical

    PropertyValue

    Transparency

    no

    Technological properties

    Property
    Application areas

    air intake sytems, electrical insulating parts, brake pedals

    Fillers

    30% Glass Fiber