Módulo elástico: 1.15 GPa

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 460

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3120-50

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850-07

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850-04

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3121-50

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3120-15

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850 PC

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850 WR

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850 Black

Suministrada por:

Arkema: High Performance Polymers

Polipropileno

Polypropylene Random Copolymer (PPR)

Suministrada por:

1 proveedor Matmatch

Polipropileno

Polypropylene Block Copolymer (PPB)

Suministrada por:

1 proveedor Matmatch

Polietileno de alta densidad (PEAD)

High Density Polyethylene (HDPE)

Suministrada por:

1 proveedor Matmatch

Polyamide 6 (PA6)

Polyamide 6 (PA6)

Suministrada por:

3 proveedores de Matmatch

Polyamide 11 (PA11)

Polyamide 11 (PA11)

Suministrada por:

1 proveedor Matmatch

Polyamide 12 (PA12)

Polyamide 12 (PA12)

Suministrada por:

1 proveedor Matmatch

Polyamide 46 (PA46)

Polyamide 46 (PA46)

Suministrada por:

1 proveedor Matmatch

Polimetilpenteno (PMP)

Polymethylpentene (PMP)

Polyamide 6/66 (PA6/66)

Copolyamide 6/66 (PA6/66)

Suministrada por:

1 proveedor Matmatch

Página 1 de 2