Description

It is a copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film and monofilaments. It is well suited for the production of nonsymetric blown film with reduced curl. Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.12 - 1.14 g/cm³

Show Material materials with Density of 1.12 - 1.14 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

1.1 - 2.2 GPa

Show Material materials with Elastic modulus of 1.1 - 2.2 GPa

Elongation

45.0 - 60.0 %

Show Material materials with Elongation of 45.0 - 60.0 %

Impact strength, Charpy notched

10.0 - 35.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 10.0 - 35.0 kJ/m²

Tensile strength

35.0 - 55.0 MPa

Show Material materials with Tensile strength of 35.0 - 55.0 MPa

at 15-25% strain

Impact strength, Charpy unnotched

no break

Thermal

PropertyValue

Coefficient of thermal expansion

7e-05 - 0.0001 1/K

Show Material materials with Coefficient of thermal expansion of 7e-05 - 0.0001 1/K

Melting point

200.0 - 260.0 °C

Show Material materials with Melting point of 200.0 - 260.0 °C

Specific heat capacity

1700 J/(kg·K)

Show Material materials with Specific heat capacity of 1700 J/(kg·K)

Thermal conductivity

0.22 W/(m·K)

Show Material materials with Thermal conductivity of 0.22 W/(m·K)

Flammability

UL 94 V2

Electrical

PropertyValue

Dielectric constant

4 [-]

Show Material materials with Dielectric constant of 4 [-]

9 [-]

Show Material materials with Dielectric constant of 9 [-]

Electrical resistivity

1000000000.0 - 10000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 1000000000.0 - 10000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

aerial housing, airbag clips, interior mirror control housing, loudspeaker grills, mobile phone consoles

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding, extrusion, blow molding