Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Cobre pudelado
CEN/TS 13388 Grade CW112C R300, H070Cobre pudelado
CEN/TS 13388 Grade CW101C R410, H090Cobre pudelado
CEN/TS 13388 Grade CW100C R410, H090Platino
Platinum (Pt)