Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Acero bajo en carbono
EN 10083-1 Grade C25E quenched and tempered (+QT)Acero bajo en carbono
EN 10083-1 Grade C25R quenched and tempered (+QT)Acero bajo en carbono
DIN 17155 Grade 17Mn4 normalized or normalized formed (+N)Molybdenum Steel
EN 10216-2 Grade 16Mo3 normalized or normalized formed (+N)Molybdenum Steel
EN 10217-2 Grade 16Mo3 normalized or normalized formed (+N)Molybdenum Steel
EN 10217-5 Grade 16Mo3 normalized or normalized formed (+N)Chromium Molybdenum Steel
EN 10216-2 Grade 13CrMo4-5 normalized and tempered (+NT)Molybdenum Steel
DIN 17155 Grade 15Mo3 normalized or normalized formed (+N)Acero bajo en carbono
EN 10083-1 Grade C25E treated for cold shearing (+S)Acero bajo en carbono
EN 10083-1 Grade C25R treated for cold shearing (+S)Nickel Chromium Molybdenum Steel
EN 10083-1 Grade 30CrNiMo8 quenched and tempered (+QT)Chromium Molybdenum Steel
EN 10083-1 Grade 34CrMo4 quenched and tempered (+QT)Nickel Chromium Molybdenum Steel
EN 10083-1 Grade 34CrNiMo6 quenched and tempered (+QT)