Elongation at yield: 2.6 %

Quick Comparison

Acrilonitrilo butadieno estireno (ABS)

Elix ABS M205FC

Suministrada por:

Elix Polymers

Acrilonitrilo butadieno estireno (ABS)

Elix ABS M203FC

Suministrada por:

Elix Polymers

Acrilonitrilo butadieno estireno (ABS)

Elix ABS H604

Suministrada por:

Elix Polymers

Acrilonitrilo butadieno estireno (ABS)

Elix ABS M203

Suministrada por:

Elix Polymers

Acrilonitrilo butadieno estireno (ABS)

CYCOLAC™ Resin X11