General
Property | Temperature | Value | Testing Standard |
---|---|---|---|
Density | 25 °C | 1.055 g/cm³ Show Supplier Material materials with Density of 1.055 g/cm³ | ISO 1183-1 |
Mechanical
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 2.5 GPa Show Supplier Material materials with Elastic modulus of 2.5 GPa | ISO 527-1/2 | 1 mm/min | |
Elongation | 15 % Show Supplier Material materials with Elongation of 15 % | ISO 527-1/2 | min. | 50 mm/min | |
Elongation at yield | 2.6 % Show Supplier Material materials with Elongation at yield of 2.6 % | ISO 527-1/2 | 50 mm/min | |
Flexural modulus | 2.6 GPa Show Supplier Material materials with Flexural modulus of 2.6 GPa | ISO 527-1/2 | 2 mm/min | |
Flexural strain | 20 % Show Supplier Material materials with Flexural strain of 20 % | ISO 527-1/2 | 50 mm/min | |
Flexural strength | 75 MPa Show Supplier Material materials with Flexural strength of 75 MPa | ISO 178 | 2 mm/min | |
Hardness, Ball Indentation | 106 MPa Show Supplier Material materials with Hardness, Ball Indentation of 106 MPa | ISO 2039-1 | ||
Impact strength, Charpy notched | -30 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m² | ISO 179-1eA | |
23 °C | 16 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m² | ISO 179-1eA | ||
Impact strength, Charpy unnotched | -30 °C | 100 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | ISO 179-1eU | |
23 °C | 124 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 124 kJ/m² | ISO 179-1eU | ||
Impact strength, Izod notched | -30 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 7 kJ/m² | ISO 180-1A | |
23 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 15 kJ/m² | ISO 180-1A | ||
Tensile strength | 36.5 MPa Show Supplier Material materials with Tensile strength of 36.5 MPa | ISO 527-1/2 | 50 mm/min | |
Yield strength | 50.5 MPa Show Supplier Material materials with Yield strength of 50.5 MPa | ISO 527-1/2 | 50 mm/min |
Thermal
Property | Value | Testing Standard | Pressure | Comment | |||
---|---|---|---|---|---|---|---|
Coefficient of thermal expansion | 7.8e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7.8e-05 1/K | ISO 11359-1/2 | 23 to 55°C | ||||
8.1e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8.1e-05 1/K | ISO 11359-1/2 | 23 to 55°C, Transverse | |||||
Glow Wire Flammability Index | 650 °C Show Supplier Material materials with Glow Wire Flammability Index of 650 °C | IEC 60695-2-12 | 2.0 mm | ||||
Heat deflection temperature | 94 °C Show Supplier Material materials with Heat deflection temperature of 94 °C | ISO 75-1/2 | 1.8 MPa | ||||
98 °C Show Supplier Material materials with Heat deflection temperature of 98 °C | ISO 75-1/2 | 0.45 MPa | |||||
Vicat softening temperature | 98 °C Show Supplier Material materials with Vicat softening temperature of 98 °C | ISO 306 | 50 N | 50°C/h | ||||
101 °C Show Supplier Material materials with Vicat softening temperature of 101 °C | ISO 306 | 50 N | 120°C/h | |||||
Flammability | At thickness 1.6 mm UL 94: HB |
Electrical
Property | Value | Frequency | Testing Standard |
---|---|---|---|
Dielectric constant | 2.82 [-] Show Supplier Material materials with Dielectric constant of 2.82 [-] | 1MHz | IEC 60250 |
3.04 [-] Show Supplier Material materials with Dielectric constant of 3.04 [-] | 100Hz | IEC 60250 | |
Dissipation factor | 0.0053 [-] Show Supplier Material materials with Dissipation factor of 0.0053 [-] | 100Hz | IEC 60250 |
0.0096 [-] Show Supplier Material materials with Dissipation factor of 0.0096 [-] | 1MHz | IEC 60250 | |
Surface resistivity | 2e+17 Ω/sq Show Supplier Material materials with Surface resistivity of 2e+17 Ω/sq | ||
Volume resistivity | 2e+16 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+16 Ω·cm | IEC 60093 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt volume-flow rate | 20 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 20 cm³/10min | ISO 1133 | 220°C/10Kg |
Shrinkage | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | ISO 2577 | 150x105x3 | 500 bar |
0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | ISO 2577 | 150x105x3 | 500 bar, Transverse |
Technological properties
Property | ||
---|---|---|
Certifications | UL Certificate | |
Handling recommendations | Please see the Material Safety Data Sheet for relevant health & safety information. | |
Other | Control measurements in other places may issue different results due to influences of machinery, equipment, test method or storage conditions. | |
Processing methods | Injection molding-melt temperature: 240 ºC according to ISO 294 Injection molding-mold temperature: 70 ºC according to ISO 294 Injection molding-injection velocity: 240 mm/s according to ISO 294 |