Mechanical
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 2.4 GPa Show Supplier Material materials with Elastic modulus of 2.4 GPa | ISO 527-1/2 | 1 mm/min | |
Elongation | 15 % Show Supplier Material materials with Elongation of 15 % | ISO 527-1/2 | min. | 50 mm/min | |
Elongation at yield | 2.6 % Show Supplier Material materials with Elongation at yield of 2.6 % | ISO 527-1/2 | 50 mm/min | |
Flexural modulus | 2.4 GPa Show Supplier Material materials with Flexural modulus of 2.4 GPa | ISO 527-1/2 | 2 mm/min | |
Flexural strength | 70 MPa Show Supplier Material materials with Flexural strength of 70 MPa | ISO 178 | 2 mm/min | |
Hardness, Ball Indentation | 110 MPa Show Supplier Material materials with Hardness, Ball Indentation of 110 MPa | ISO 2039-1 | ||
Impact strength, Charpy notched | -30 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m² | ISO 179-1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m² | ISO 179-1eA | ||
Impact strength, Charpy unnotched | -30 °C | 90 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m² | ISO 179-1eU | |
23 °C | 110 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 110 kJ/m² | ISO 179-1eU | ||
Impact strength, Izod notched | -30 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 7 kJ/m² | ISO 180-1A | |
23 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 15 kJ/m² | ISO 180-1A | ||
Yield strength | 46 MPa Show Supplier Material materials with Yield strength of 46 MPa | ISO 527-1/2 | 50 mm/min |
Thermal
Property | Value | Testing Standard | Pressure | Comment | |||
---|---|---|---|---|---|---|---|
Coefficient of thermal expansion | 9e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9e-05 1/K | ISO 11359-1/2 | 23 to 55°C | ||||
Glow Wire Flammability Index | 700 °C Show Supplier Material materials with Glow Wire Flammability Index of 700 °C | IEC 60695-2-12 | 2.0 mm | ||||
Heat deflection temperature | 94 °C Show Supplier Material materials with Heat deflection temperature of 94 °C | ISO 75-1/2 | 1.8 MPa | ||||
98 °C Show Supplier Material materials with Heat deflection temperature of 98 °C | ISO 75-1/2 | 0.45 MPa | |||||
Vicat softening temperature | 99 °C Show Supplier Material materials with Vicat softening temperature of 99 °C | ISO 306 | 50 N | 50°C/h | ||||
Flammability | At thickness 1.6 mm UL 94: HB. Burning rate US-FMVSS (200x105x2 mm): 60 mm/min according to ISO 3795 |
Electrical
Property | Value | Testing Standard | Frequency | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | IEC 60112 | Solution A | |
Dielectric constant | 2.9 [-] Show Supplier Material materials with Dielectric constant of 2.9 [-] | IEC 60250 | 1MHz | |
3 [-] Show Supplier Material materials with Dielectric constant of 3 [-] | IEC 60250 | 100Hz | ||
Dielectric strength | 35 kV/mm Show Supplier Material materials with Dielectric strength of 35 kV/mm | IEC 60243-1 | 1 mm | |
Dissipation factor | 0.005 [-] Show Supplier Material materials with Dissipation factor of 0.005 [-] | IEC 60250 | 100Hz | |
0.008 [-] Show Supplier Material materials with Dissipation factor of 0.008 [-] | IEC 60250 | 1MHz | ||
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | |||
Volume resistivity | 1e+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+15 Ω·cm | IEC 60093 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt volume-flow rate | 31 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 31 cm³/10min | ISO 1133 | 220°C/10Kg |
Shrinkage | 0.4 - 0.7 % Show Supplier Material materials with Shrinkage of 0.4 - 0.7 % | ISO 294-4 | 60x60x2 mm |
0.4 - 0.7 % Show Supplier Material materials with Shrinkage of 0.4 - 0.7 % | ISO 294-4 | 60x60x2 mm, Transverse |
Technological properties
Property | ||
---|---|---|
Certifications | UL Certificate | |
Handling recommendations | Please see the Material Safety Data Sheet for relevant health & safety information. | |
Other | Control measurements in other places may issue different results due to influences of machinery, equipment, test method or storage conditions. | |
Processing methods | Injection molding-melt temperature: 240 ºC according to ISO 294 Injection molding-mold temperature: 70 ºC according to ISO 294 Injection molding-injection velocity: 240 mm/s according to ISO 294 |