Módulo de flexión: 21 GPa

Quick Comparison

Polyamide 46 (PA46)

Stanyl® TW272B6

Suministrada por:

DSM Engineering Materials

Polyphenylene Sulfide (PPS)

PPS GF65 MD SGM651E43

Suministrada por:

Shandong Sciengy New Materials Co. Ltd

Polyphenylene Sulfide (PPS)

PPS CF30 SGC301S87

Suministrada por:

Shandong Sciengy New Materials Co. Ltd