General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density | 1.36 g/cm³ Show Supplier Material materials with Density of 1.36 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.2 % Show Supplier Material materials with Moisture absorption of 2.2 % | dry | Sim. to ISO 62 | |
Water absorption | 2.25 % Show Supplier Material materials with Water absorption of 2.25 % | dry | ISO 62 | at 23°C after 24h |
8.1 % Show Supplier Material materials with Water absorption of 8.1 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | -40 °C | 23.5 GPa Show Supplier Material materials with Elastic modulus of 23.5 GPa | dry | ISO 527-1/-2 |
14.5 GPa Show Supplier Material materials with Elastic modulus of 14.5 GPa | conditioned | ISO 527-1/-2 | ||
23.5 GPa Show Supplier Material materials with Elastic modulus of 23.5 GPa | dry | ISO 527-1/-2 | ||
120 °C | 12.5 GPa Show Supplier Material materials with Elastic modulus of 12.5 GPa | dry | ISO 527-1/-2 | |
160 °C | 11 GPa Show Supplier Material materials with Elastic modulus of 11 GPa | dry | ISO 527-1/-2 | |
180 °C | 10.5 GPa Show Supplier Material materials with Elastic modulus of 10.5 GPa | dry | ISO 527-1/-2 | |
200 °C | 10 GPa Show Supplier Material materials with Elastic modulus of 10 GPa | dry | ISO 527-1/-2 | |
Elongation | -40 °C | 1.5 % Show Supplier Material materials with Elongation of 1.5 % | dry | ISO 527-1/-2 |
1.6 % Show Supplier Material materials with Elongation of 1.6 % | dry | ISO 527-1/-2 | ||
3.5 % Show Supplier Material materials with Elongation of 3.5 % | conditioned | ISO 527-1/-2 | ||
120 °C | 3.1 % Show Supplier Material materials with Elongation of 3.1 % | dry | ISO 527-1/-2 | |
160 °C | 3.1 % Show Supplier Material materials with Elongation of 3.1 % | dry | ISO 527-1/-2 | |
180 °C | 3.1 % Show Supplier Material materials with Elongation of 3.1 % | dry | ISO 527-1/-2 | |
200 °C | 3.1 % Show Supplier Material materials with Elongation of 3.1 % | dry | ISO 527-1/-2 | |
Flexural modulus | 12.5 GPa Show Supplier Material materials with Flexural modulus of 12.5 GPa | conditioned | ISO 178 | |
21 GPa Show Supplier Material materials with Flexural modulus of 21 GPa | dry | ISO 178 | ||
120 °C | 10.5 GPa Show Supplier Material materials with Flexural modulus of 10.5 GPa | dry | ISO 178 | |
160 °C | 10 GPa Show Supplier Material materials with Flexural modulus of 10 GPa | dry | ISO 178 | |
Flexural yield strength | 240 MPa Show Supplier Material materials with Flexural yield strength of 240 MPa | conditioned | ISO 178 | |
340 MPa Show Supplier Material materials with Flexural yield strength of 340 MPa | dry | ISO 178 | ||
120 °C | 200 MPa Show Supplier Material materials with Flexural yield strength of 200 MPa | dry | ISO 178 | |
160 °C | 170 MPa Show Supplier Material materials with Flexural yield strength of 170 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 8 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 50 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 50 kJ/m² | dry | ISO 179/1eU |
-30 °C | 55.0 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 55.0 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 50 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 50 kJ/m² | dry | ISO 179/1eU | |
23 °C | 80 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 80 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | -40 °C | 265 MPa Show Supplier Material materials with Tensile strength of 265 MPa | dry | ISO 527-1/-2 |
160 MPa Show Supplier Material materials with Tensile strength of 160 MPa | conditioned | ISO 527-1/-2 | ||
250 MPa Show Supplier Material materials with Tensile strength of 250 MPa | dry | ISO 527-1/-2 | ||
120 °C | 130 MPa Show Supplier Material materials with Tensile strength of 130 MPa | dry | ISO 527-1/-2 | |
160 °C | 110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | dry | ISO 527-1/-2 | |
180 °C | 100 MPa Show Supplier Material materials with Tensile strength of 100 MPa | dry | ISO 527-1/-2 | |
200 °C | 90 MPa Show Supplier Material materials with Tensile strength of 90 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 2.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
3.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Glass transition temperature | 75 °C Show Supplier Material materials with Glass transition temperature of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Heat deflection temperature | 290 °C Show Supplier Material materials with Heat deflection temperature of 290 °C | dry | ISO 75-1/-2 | 2 MPa | |
Melting point | 295 °C Show Supplier Material materials with Melting point of 295 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Shrinkage | 0.3 % Show Supplier Material materials with Shrinkage of 0.3 % | dry | ISO 294-4 | Parallel |
0.6 % Show Supplier Material materials with Shrinkage of 0.6 % | dry | ISO 294-4 | Normal | |
Viscosity number | 150 cm³/gr Show Supplier Material materials with Viscosity number of 150 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 30% Carbon Fiber and PTFE |