Módulo de flexión: 14.5 GPa

Quick Comparison

Polyamide 4T (PA4T)

ForTii® F12

Suministrada por:

DSM Engineering Materials

Polyphenylene Sulfide (PPS)

Xytron™ G4010T

Suministrada por:

DSM Engineering Materials

Polyphenylene Sulfide (PPS)

Xytron™ G4012T

Suministrada por:

DSM Engineering Materials

Polyamide 4T (PA4T)

ForTii® MX2

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF00AS

Suministrada por:

Sabic

Polyphenylene Sulfide (PPS)

Xytron™ G4010W

Suministrada por:

DSM Engineering Materials

Other Polyamide (PA)

Akulon® GA-XLG0

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

EPLAMID 66 GFS 50 HS NC Q1F001 (PA66)

Suministrada por:

EPSAN

Polyamide 66 (PA66)

EPLAMID 66 GFU 50 UVH BK Q1F001 (PA66)

Suministrada por:

EPSAN

Polyamide 6 (PA6)

EPLAMID 6 GFR 50 NC Q1F001 (PA6)

Suministrada por:

EPSAN

Polyamide 46 (PA46)

Stanyl® 46HF5145

Suministrada por:

DSM Engineering Materials

Polietileno tereftalato (PET)

VYPET™ VNT-645

Suministrada por:

Lavergne

Polyphenylene Sulfide (PPS)

PPS GF40

Suministrada por:

Xiamen Keyuan Plastic Co., Ltd