PPS GF40

Alternative and trade names
PPS-GF40
Want to keep this datasheet? Save it now in your required format

Description

Polyphenylene Sulfide (PPS) reinforced with 40% glass fiber

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.62 g/cm³

Show Supplier Material materials with Density of 1.62 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

14.5 GPa

Show Supplier Material materials with Flexural modulus of 14.5 GPa

ASTM D790

Flexural strength

23.0 °C

200 MPa

Show Supplier Material materials with Flexural strength of 200 MPa

ASTM D790

Hardness, Shore D

23.0 °C

84 [-]

Show Supplier Material materials with Hardness, Shore D of 84 [-]

ASTM D785

Impact strength, Charpy notched, ASTM

23.0 °C

80 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 80 J/m

ASTM D256

Tensile strength

23.0 °C

179 MPa

Show Supplier Material materials with Tensile strength of 179 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature

279 °C

Show Supplier Material materials with Heat deflection temperature of 279 °C

ASTM D648

Electrical

PropertyTemperatureValueComment

Dielectric constant

23.0 °C

3.8 [-]

Show Supplier Material materials with Dielectric constant of 3.8 [-]

ASTM D147

Dielectric strength

23.0 °C

20 kV/mm

Show Supplier Material materials with Dielectric strength of 20 kV/mm

ASTM D147

Surface resistivity

23.0 °C

1.00E+16 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+16 Ω/sq

ASTM D257

Technological properties

Property
Application areas

Automotive bumpers, Automotive applications, Automotive exterior parts

Fillers

40% Glass Fiber