Acero bajo en carbono
EN 10025-3 Grade S420N normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10025-3 Grade S420NL normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10025-2 Grade S235JR as-rolled condition (+AR)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10225 Grade S420G1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S460M thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Acero inoxidable austenítico
ASTM A276 Grade S20910 AnnealedAcero inoxidable ferrítico
SEW 400 Grade X20CrMo13 quenched and tempered (+QT)Acero inoxidable martensítico
SEW 400 Grade X4CrNi13-4 quenched and tempered (+QT1)Acero inoxidable ferrítico
EN 10088-1 Grade X2CrNi12 quenched and tempered (+QT)Wrought Copper High Copper Alloy
EN 1652 Grade CuBe2 THChromium Molybdenum Steel
DIN 17240 Grade 21CrMoV5-7 quenched and tempered (+QT)Acero inoxidable ferrítico
DIN 17442 Grade X20CrMo13 quenched and tempered (+QT)Acero inoxidable martensítico
SEW 400 Grade X35CrMo17 quenched and tempered (+QT)Wrought Copper Nickel Silver Grade
Niclafor® 1000 TD4 - (Strips, Sheets) - CuNi9Sn6 - C72700Suministrada por:
Lebronze Alloys