Ductile (Nodular) Cast Iron
EN 1564 Grade GJS-1200-2 austemperedWrought Copper High Copper Alloy
EN 12166 Grade CuBe2Pb H350Wrought Copper High Copper Alloy
EN 12165 Grade CuBe2 MChromium Molybdenum Steel
DIN 1.7734 6Wrought Copper High Copper Alloy
EN 12163 Grade CuBe2 MAcero de alto carbono
ASTM A551 Class DHT Heat-TreatedWrought Copper High Copper Alloy
EN 12163 Grade CuBe2 H350Wrought Copper High Copper Alloy
EN 12166 Grade CuBe2 H350Wrought Copper High Copper Alloy
EN 1652 Grade CuBe2 H340Wrought Copper High Copper Alloy
EN 12163 Grade CuBe2 F00Ductile (Nodular) Cast Iron
EN 1564 Grade GJS-1400-1 cast conditionAcero inoxidable martensítico
ASTM A693 Grade XM-12 Solution-TreatedAcero inoxidable martensítico
ASTM A705 Grade XM-12 Solution Annealed