Heat deflection temperature, 0.45 MPa: 208 °C

Quick Comparison

Polieterimida (PEI)

ULTEM™ Resin UF5011S - Europe

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin UF5011S - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin UF5011S - Americas

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin CRS5011R - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin CRS5011R - Europe

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin CRS5011R - Americas

Suministrada por:

Sabic

Polyamide 6 (PA6)

LNP™ KONDUIT™ Compound PX11311U

Suministrada por:

Sabic