General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.74 g/cm³ Show Supplier Material materials with Density of 1.74 g/cm³ | ISO 1183 |
Water absorption | 23.0 °C | 0.36 % Show Supplier Material materials with Water absorption of 0.36 % | ISO 62-1 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 12 GPa Show Supplier Material materials with Elastic modulus of 12 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 1.7 % Show Supplier Material materials with Elongation of 1.7 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 11 GPa Show Supplier Material materials with Flexural modulus of 11 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 170 MPa Show Supplier Material materials with Flexural strength of 170 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 3 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 25 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Tensile strength | 23.0 °C | 105 MPa Show Supplier Material materials with Tensile strength of 105 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 165°C +/- 2°C | |||
Coefficient of thermal expansion | 23.0 °C | 3.72E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.72E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6.04E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6.04E-5 1/K | ISO 11359-2 | -30°C to 80°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | IEC 60695-2-13 | 1.6 mm | |||
Heat deflection temperature | 185 - 208 °C Show Supplier Material materials with Heat deflection temperature of 185 - 208 °C | ||||
Heat deflection temperature, 0.45 MPa | 208 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 208 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 185 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 185 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 120 °C Show Supplier Material materials with Relative temperature index, electrical of 120 °C | UL 746B | |||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Thermal conductivity | 23.0 °C | 1.3 W/(m·K) Show Supplier Material materials with Thermal conductivity of 1.3 W/(m·K) | ISO 22007-2 | ?80*3mm discs | ||
Thermal conductivity, through-plane | 23.0 °C | 1.1 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 1.1 W/(m·K) | ISO 22007-2 | ?80*3mm discs | ||
Vicat softening temperature | 205 °C Show Supplier Material materials with Vicat softening temperature of 205 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101761336- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥1mm UL 94 <br> Glow Wire Ignitability Temperature, 1.0 mm: 800°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 775°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 0 V Show Supplier Material materials with Comparative tracking index of 0 V | UL 746A | (UL) {PLC} |
Dielectric strength | 23.0 °C | 15.9 kV/mm Show Supplier Material materials with Dielectric strength of 15.9 kV/mm | ASTM D 149 | in oil, 1.6 mm |
High Amp Arc Ignition | 23.0 °C | 1 mm Show Supplier Material materials with High Amp Arc Ignition of 1 mm | ≥, UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 1 mm Show Supplier Material materials with Hot-Wire Ignition of 1 mm | ≥, UL 746A | PLC 0 |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | LED Lighting | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |